1. What is the die bore clearance between punch and die in mm, and how do you measure it?
Measure diametral clearance, not the gap you can see by eye: subtract the punch tip outside diameter from the die bore inside diameter. Both readings come from the same micrometer session — tip with an outside micrometer, bore with a bore gauge or inside micrometer — and the difference is the number the tooling designer actually works with.
|
Diametral clearance |
Per side |
What the press gives you |
|
Below 0.02 mm |
Below 0.01 mm |
Tip pickup, scoring, seizure on a warm press |
|
0.02–0.05 mm |
0.01–0.025 mm |
Running clearance with a controlled edge |
|
Above 0.05 mm |
Above 0.025 mm |
Flash, burr, weight drift, early die wear |
The five-point measurement
- Clean both surfaces. A gram of compacted powder on the die land reads as a tighter bore than reality.
- Measure the punch tip at three heights, two axes. Six readings; record the smallest and largest.
- Measure the bore at the entry, the compression zone and the exit, two axes each. This is where die bore wear symptoms and measurement stop being theory: a bore that reads 0.02 mm bigger at the entry than in the compression zone is bell-mouthed from years of punch entry, not out of tolerance.
- Subtract like for like. Bore ID minus tip OD = diametral clearance. Compare with the largest tip reading and the smallest bore reading — that is the worst case your press will see, not the average.
- Track the trend, not one number. Record clearance at every die change. When it doubles from the as-new value, plan replacement. A step change in one station points to that die, not to your granulation.
A shop-floor shortcut is a go/no-go plug gauge at 0.02 and 0.05 mm: fast enough for every die at changeover, but it only tells you which band you are in, not that the bore has gone oval. Use the gauge for screening and the bore gauge for decisions. Keante ships each die with its bore reading and the matched tip OD printed on the label, so the die bore clearance between punch and die in mm is already calculated when the box arrives.
✅ Bottom line: Diametral clearance is bore ID minus tip OD; measure both on three levels and two axes, and treat a doubling from the as-new value as a replacement trigger.

2. What does flash and burr on tablet edge die clearance actually cost?
Too much clearance lets the granulation take the path around the tablet instead of forming it: the annular gap becomes a mould for a thin fin. On an 18 mm punch tip at 0.05 mm diametral clearance, the radial gap is 0.025 mm and the escape annulus is π × 18 × 0.025 ≈ 1.4 mm² — about 0.55% of the tablet face. That sounds negligible until peak pressure pushes the fines through it thousands of times a minute. The result is flash and burr on tablet edge die clearance — a hairline fringe that breaks off, scuffs the die wall and returns as black specks in the next tablets.
Read the defect to find the end you are on
- Flash all around, growing slowly: clearance above 0.05 mm across the bore, usually from a worn die. Replace the die, not the punch.
- Flash on one side only: bell-mouthed entry or a punch entering off-axis. Check the bore at three heights, then check the barrel and the guide bore before blaming clearance.
- Scoring on the punch tip, rising ejection force, a punch that will not withdraw: clearance below 0.02 mm. The tip is rubbing the bore; stop the press before the head is damaged.
- Tablet diameter creeping up station by station: the die bore is wearing oval, and the clearance budget is being spent unevenly around the circumference.
The tight end is the expensive one. A seized punch does not just scrap tablets: it loads the head against the roller and can take out a cam segment, so a few cents of clearance turns into a full station inspection. The loose end is cheaper per event but continuous — a deburring step, a rejected batch, and a die that never reaches its rated life. Both are prevented by the same five readings.
This is where die bore wear symptoms and measurement become a purchasing question rather than a maintenance one. A custom tooling order that specifies only "B round, 18 mm" leaves the clearance to the shop that quotes it. State the tip OD, the bore ID and the resulting clearance on the drawing, ask your supplier for the as-new reading with the goods, and reject a batch whose clearance sits at the edge of the band — Keante holds production dies in the middle of the band rather than at its limits, because the middle is where both failure modes stay quiet.
✅ Bottom line: Flash means clearance too wide, tip scoring means too narrow; specify tip OD and bore ID on the drawing and keep both in the middle of the band.

FAQ
Q: Is 0.05 mm too loose for a 6 mm tablet? A: Yes. Keep small tips at the low end of the band: 0.02 mm diametral or tighter, provided the turret is in good alignment. The same 0.05 mm gap that is harmless on an 18 mm tip is a much larger fraction of a 6 mm face, so the fin becomes a visible part of the tablet rather than a trace.
Q: Can a worn die be reamed back to size? A: No — reaming removes metal from the bore, so it increases clearance and makes the flash worse. A bell-mouthed or oval bore is replaced, or relined with a pressed-in insert by a shop equipped for it. Re-polishing is fine for a light score, provided the bore is checked again on both axes.
Q: What is the first sign that clearance has drifted out of band? A: Flash appearing on one edge of the tablet, before weight or hardness moves. Follow it with a bore reading at three heights: a 0.02–0.03 mm increase at the entry alone means bell-mouthing, while an even increase all through the bore means general wear. Keante includes the three-height bore reading with every replacement die, so the baseline is on the label from day one.
CTA: Get the clearance written on the drawing
Send the tablet diameter, press model and current punch tip reading, and Keante returns a die specification with bore ID, diametral clearance and the target band filled in — plus a wear baseline to compare against at every changeover. Keante (Shandong) Intelligent Equipment Co., Ltd. is a China manufacturer of compression tooling, supplying OEM and wholesale punches and dies with paired measurements, from single spare parts to full turret sets.
|
|
|
|
Published: November 2026 |